Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 132.4 MPa | 19210 psi | ASTM D638 |
E-Polymers SEPAZ® LH50 PP Homopolymer LFT Resin Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver.. |
|||
Tensile Strength | 132.4 MPa | 19210 psi | ASTM D638 |
E-Polymers SEPAZ® C130GP 30% Glass Fiber Reinforced LCP Resin Liquid Crystal Polymer Resin: SEPAZ LCP resin has a unique structure and performance unthought of in a traditional plastics. Beside SEPAZ LCP takes the excels in all-around performance and molding .. |