Mechanical Properties Metric English Comments
Tensile Strength 2.80 MPa
406 psi
ISO 37 Type 2
Rogers Corporation Bisco® A2 Sound Barrier Engineered Solid Silicone Mass Layer, Sound Barrier
BISCO® A2 Sound Barrier is a solid silicone rubber engineered to meet demanding requirements for flammability, smoke density and toxicity. A2 is used to block the transmission of sound and demonst..
Tensile Strength 2.80 MPa
406 psi
Shin-Etsu Silicones LIMSâ„¢ KE2004-10A/B Elastomer
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 2.80 MPa

@Strain 20.0 %
406 psi

@Strain 20.0 %
ISO 37
BASF Elastollan 685 AU TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength 2.80 MPa
406 psi
20; ISO 37
BASF Elastollan 880 AN TPUR
Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien..
Tensile Strength 2.80 MPa
406 psi
ISO 37
AlphaGary Evoprene™ GC 5697 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..