Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 20.24 MPa | 2935 psi | Product Property; Arlon SQA-TMS-048 |
Arlon T3020-R004 0.020" (0.508 mm) Thick, 1" wide, Cured Fusible Silicone Rubber with Sinusoidal Fiberglass Substrate Design/Construction: Side 1: Cured Fusible Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Fusible Silicone Rubber Interleave: Polyester FilmArlon MOX-Tape® Fiberglass Reinforced T.. |