Mechanical Properties Metric English Comments
Tensile Strength 1.43 MPa

@Temperature 22.0 °C,
Time 252000 sec
207 psi

@Temperature 71.6 °F,
Time 70.0 hour
50% RH, Exposure to Carpet Cleaner; ASTM D412
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi..
Tensile Strength 1.43 MPa

@Temperature 22.0 °C,
Time 252000 sec
207 psi

@Temperature 71.6 °F,
Time 70.0 hour
50% RH, Exposure to Hairspray; ASTM D412
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi..
Tensile Strength 1.43 MPa

@Temperature 22.0 °C,
Time 252000 sec
207 psi

@Temperature 71.6 °F,
Time 70.0 hour
50% RH, Exposure to Windshield Washer Solvent; ASTM D412
Parker Chomerics CHO-SEAL S6305 Conductive Elastomer
Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact.Molded and Extruded.RoHS CompliantInformation provi..