Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 23.2 MPa @Strain 100 % |
3360 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A6DE3 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |