Polymer Property : Tensile Strength = 2320 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 16.0 MPa
>= 2320 psi
Type IV, 500mm/min; ASTM D638
S&E Specialty Polymers SE900-5 PVC
Description: PVC weatherable, integral colored, filledApplications: Roof Ditch Molding Core which meets the Ford WSKM4D689-A4Information provided by S&E Specialty Polymers
Tensile Strength 16.0 MPa
2320 psi
ISO 527
Premix Thermoplastics PRE-ELEC® ESD 5350 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5350 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val..
Tensile Strength 16.0 MPa
2320 psi
ISO 527
Premix Thermoplastics PRE-ELEC® ESD 5360 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5360 is a static dissipative thermoplastic compounds based on polypropylene homopolymer. The dissipative property is permanent and built into the polymer chain. Surface resistance val..
Tensile Strength 16.0 MPa
2320 psi
ISO 527
Premix Thermoplastics PRE-ELEC® ESD 5500 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 5500 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5500 can be injectio..
Tensile Strength 16.0 MPa
2320 psi
ISO 527
Premix Thermoplastics PRE-ELEC® ESD 6610 Static Dissipative Thermoplastic Compound
PRE-ELEC® ESD 6610 is a static dissipative thermoplastic compound based on high impact polystyrene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 6610 has b..
Tensile Strength >= 16.0 MPa
>= 2320 psi
DIN 53504
NEXA® PFX9010 Perfluoroelastomer
NEXA produces sealing elements for extreme and critical applications, particularly where high temperature, wet conditions (steam/water), purity and chemical resistance are important factors to consi..
Tensile Strength 16.0 MPa
2320 psi
at Yield; ISO 527-1/-2
Quadrant EPP TIVAR® Burnguard PE-UHMW + flame retardant + other additives (ISO Data)
TIVAR Burnguard is a PE-UHMW grade containing a very effective non-halogenated flame retardant. Specifically developed to improve the poor flammability behaviour of straight forward virgin polyethyl..
Tensile Strength 16.0 MPa
2320 psi
at Yield; ISO 527-1/-2
Quadrant EPP TIVAR® Oil Filled PE-UHMW + oil (ISO Data)
TIVAR Oil Filled is a self-lubricating PE-UHMW material in the real meaning of the word. Next to an enhanced wear resistance, the incorporated and evenly dispersed oil renders this material a consid..
Tensile Strength 16.0 MPa
2320 psi
ASTM D2095
Permabond UV620 UV-curable Adhesive
PERMABOND UV620 is a single part, fast curing, UV curable adhesive. Its excellent optical clarity and resistance to yellowing make it ideal for bonding glass and crystal for a high quality finish. I..
Tensile Strength 16.0 MPa
2320 psi
ISO 37
Kraton® D4271 J (O/E SBS) Branched Block Copolymer
Description: Kraton D4271 J is an oil-extended branched block copolymer based on styrene and butadiene, with bound styrene of 45% mass. It is supplied from Japan in the physical forms identified in ..
Tensile Strength 16.0 MPa
2320 psi
Average; ASTM D412 Method A
Seals Eastern 5794 Fluorocarbon-Elastomer
Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type..
Tensile Strength 16.0 MPa
2320 psi
ASTM D412
Wanhua Chemical Wanthane® WHT-A885 Aliphatic TPU
Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd.
Tensile Strength 16.0 MPa

@Strain 100 %
2320 psi

@Strain 100 %
ISO 37
BASF Elastollan B 60 D TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup..
Tensile Strength >= 16.0 MPa
>= 2320 psi
ISO 37
Austin Novel Materials Texalan® 365A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tensile Strength 16.0 MPa

@Strain 100 %
2320 psi

@Strain 100 %
ISO 37
BASF Elastollan S 98 A TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength >= 16.0 MPa
>= 2320 psi
ISO 37
Austin Novel Materials Texalan® 665A Polyester and Polyether based TPU
Description: A kind of custom-made products which use different raw materials to meet customers special requirementsInformation from Dawnentech