Polymer Property : Tensile Strength = 24400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 168 MPa
24400 psi
5.0 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)  (Unverified Data**)
AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra..
Tensile Strength 168 MPa
24400 psi
5 mm/min; ASTM D638
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable..