Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 0.172 MPa
25.0 psi
ASTM D412
Rogers Corporation Bisco® BF-2000 Ultra-Soft Silicone Foam
BISCO® Ultra Soft is a highly compressible silicone foam. The combination of low weight and softness makes this flame retardant foam ideal for transportation, industrial and electronics applicatio..