Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 26.00 MPa | 3770 psi | ASTM D882 |
E-Polymers EFLEX® I1020 Ionomer I-series (Ionomer): E-FLEX Ionomer is a family of ethylene acrylic acid (E/AA) copolymers, in which part of the acrylic acid is neutralized with metal ions such as zinc (Zn) or sodium (Na) or magnes.. |