Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 261 MPa | 37900 psi | |
COI Ceramics Nextel™ AS-N650 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |