Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 182 MPa | 26500 psi | 50 mm/min; ISO 527-1,-2 |
Gromax BFG30-B103N1 Nylon 6 33% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 182 MPa | 26500 psi | 50 mm/min; ISO 527 |
Gromax CFG35-R113N1 Nylon 6 36% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 183 MPa | 26500 psi | ASTM D638 |
Teknor Apex Chemlon® 345G Nylon 610, Glass Fiber Reinforced Processing Method: Injection Molding Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength | 183 MPa | 26500 psi | ASTM D-638 |
PlastiComp Complet® LGF30 - PA66 Nylon 66, 30% Long Glass Fiber Reinforced Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 66 with 30% long glass fiber reinforcementInformation provided by PlastiComp, In.. |