Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 27.9 MPa | 4050 psi | ISO 527 |
MRC Polymers MAXTEL™ 630-BK Polypropylene Copolymer • For extrusion applications• Excellent process ability.Information provided by MRC Polymers Inc. |
|||
Tensile Strength | 27.9 MPa | 4050 psi | ASTM D412 |
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound – High hardnessUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are requiredAvailable in Americas, E.. |