Polymer Property : Tensile Strength = 2726.0 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 18.795 MPa

@Temperature 121 °C,
Time 605000 sec
2726.0 psi

@Temperature 250 °F,
Time 168 hour
Air Oven Aging
S&E Specialty Polymers TufFlex™ GA-509-80-5 TPE Compound
Application: A Matte Finish, Flexible, Sunlight Resistant, 105?C Jacketing Compound with 60?C Oil Resistance.Information provided by S&E Specialty Polymers