Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 28.3 MPa | 4100 psi | ASTM D412 |
Northstar Polymers MGP-D50A High Performance Polyurethane Cast Elastomer System 50D This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires some load-bearing, slide abrasion, constant water contac.. |
|||
Tensile Strength | 28.3 MPa | 4100 psi | 2 in/min; ASTM D638 |
Braskem TR3350CW Random Copolymer Polypropylene Description: Excellent mold release, superior color and processing stability, high melt flow, excellent processability, clarified.Applications: Suggested uses include housewares, fast-cycle injectio.. |
|||
Tensile Strength | 28.3 MPa | 4100 psi | ASTM D638 |
Aaron Industries AAROLENE® ARPE HD 300-2 High Density Polyethylene Compounded Resin AAROLENE® ARPE 300 Series Polyethylene Compounded Resin HDPEColor may be specified. Melt Flow Index may be specified. Specific Gravity may be specified. |
|||
Tensile Strength | 28.3 MPa | 4100 psi | ASTM D638 |
Aaron Industries AAROLENE® ARPP H 200-1 Polypropylene Compounded Resin AAROLENE® ARPP 200 Series Polypropylene Compounded ResinColor may be specified. Melt Flow Index may be specified. |