Mechanical Properties Metric English Comments
Tensile Strength 2800 MPa
406000 psi
COI Ceramics Nicalon™ HI SiC Low O Ceramic Fiber
Description: Manufactured near-oxygen-free using electron-beam curing. The fiber is homogeneously composed of ultrafine beta-SiC crystallites and carbon. The fiber has excellent strength and modulus..
Tensile Strength 2800 MPa
406000 psi
COI Ceramics Nicalon™ HRV SiCO Ceramic Fiber
Description: The fiber is homogeneously composed of ultra-fine beta-SiC crystallites and an amorphous mixture of silicon, carbon, and oxygen. The fiber has excellent strength and modulus properties ..