Polymer Property : Tensile Strength = 2883 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 19.88 MPa

@Treatment Temp. 100 °C,
Time 605000 sec
2883 psi

@Treatment Temp. 212 °F,
Time 168 hour
Oven aged
S&E Specialty Polymers GA-3133S-CCUV PVC
Application: Meets style 1277 T.C. Power & Control Cable Requirements and can be used for CM(X), CATV(X) and CL2 jacketing applications. UL listed for 720hr. sunlightInformation provided by S&E Spec..