Mechanical Properties Metric English Comments
Tensile Strength 3.30 MPa
478 psi
ASTM D412
Northstar Polymers MPA-A30B Mold-Making Resin
MPA-A30B is a room-temperature-cure liquid castable polyurethane system. This ether-base polyurethane system is used in applications such as mold-making, prototyping, production of cast parts, pott..
Tensile Strength 3.30 MPa

@Strain 300 %
479 psi

@Strain 300 %
ISO 37
BASF Elastollan S 50 A SPF TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tensile Strength 3.30 MPa
479 psi
ISO 37
AlphaGary Evoprene™ 047 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
Tensile Strength 3.30 MPa
479 psi
average; perpendicular to plane; ASTM C297
3A Composites Core Materials AIREX® T92.130 Easy Processing Structural Foam
AIREX® T92 is a closed-cell, thermoplastic and recyclable polymer foam with very good mechanical properties and price / performance ratio. It has a good resistance to fatigue, is chemically stable,..
Tensile Strength 3.30 MPa
479 psi
ISO 37
AlphaGary Evoprene™ GC 5654 SEBS Thermoplastic Elastomer
Evoprene™ GC compounds are based on styrene ethylene- butylene styrene block copolymers. Evoprene™ GC series was created to provide cost effective solutions for processors and end users alike. Can..
Tensile Strength 3.30 MPa

@Strain 100 %
479 psi

@Strain 100 %
ISO 37
BASF Elastollan S 70 A SPF TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..