Mechanical Properties Metric English Comments
Tensile Strength 3.40 MPa
493 psi
Shin-Etsu Silicones KE-1833 Silicone, RTV Adhesive/Sealant
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 3.40 MPa
493 psi
ISO 37
AlphaGary Evoprene™ 036 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..