Mechanical Properties Metric English Comments
Tensile Strength 21.1 MPa
3060 psi
ISO 527
Murtfeldt Material ”S”® 8000 Polyethylene
Material ”S”® 8000 improves on the already impressive material properties of Original Material ”S”®. The self lubricating character of this material makes it ideally suited for use in sliding..