Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 21.6 MPa | 3130 psi | ISO 527 |
Murtfeldt Original Material ”S”® plus + Bright ESD Polyethylene, Conductive Material ”S”® plus+ Bright ESD is a light plastic with high conductivity and a voltage-dissipating effect on earthed components. This material is ideal for use in applications where a high value.. |
|||
Tensile Strength | >= 21.6 MPa | >= 3130 psi | Cure: 40 mins at 135°C; ISO 37 |
Kraton® Cariflex™ IR0307 K Polyisoprene Description: Cariflex IR0307 KU polymer is a solution polymerized polyisoprene with a high cis-1,4 content. It has a high molecular weight as indicated by its Logarithmic Inherent Viscosity (LIV) va.. |
|||
Tensile Strength | >= 21.6 MPa | >= 3130 psi | Cure: 40 mins at 135°C; ISO 37 |
Kraton® Cariflex™ IR0310 K Polyisoprene Description: Cariflex IR0310 KU polymer is a solution polymerized polyisoprene with a high cis-1,4 content. It has a high molecular weight as indicated by its Logarithmic Inherent Viscosity (LIV) va.. |
|||
Tensile Strength | >= 21.6 MPa | >= 3130 psi | Cure: 40 mins at 135°C; ISO 37 |
Kraton® IR307 Polyisoprene Description: Kraton IR307 polymer is a solution polymerized polyisoprene with a high cis-1,4 content. It has a high molecular weight as indicated by its limiting viscosity number of 7.75 dl/g. Regi.. |
|||
Tensile Strength | 21.6 MPa | 3130 psi | |
Taiwan Sheen Soon Sheenthane® A7530 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 21.6 MPa | 3130 psi | |
Taiwan Sheen Soon Sheenthane® A8631N Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 21.6 MPa | 3130 psi | ASTM D638M |
Asia Technology Pioneers CAP 501 PP Nanocomposite Description: CAP501 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective.Advantages:Good paint abilityGood dim.. |
|||
Tensile Strength | 21.6 MPa | 3130 psi | ASTM D638M |
Asia Technology Pioneers CAP 702 PP Nanocomposite Description: CAP702 is a hi-tech compounded polypropylene. This Hi-composite is produced by Nano-Technology and used widely in industry and is so cost effective. Advantages:Good paint abilityGood di.. |