Tensile Strength 21.9 MPa
3180 psi
ISO 527
S&E Specialty Polymers TufFillâ„¢ 5701 Black PP
Application: High Calcium carbonate filed, high heat resistance thermoplastic extrusion grade based on polypropylene copolymer/homopolymer.Information provided by S&E Specialty Polymers