Polymer Property : Tensile Strength = 3230 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 22.3 MPa
3230 psi
After Heat Aging 168 hrs at 150°C; ASTM D412
Kraton® G7820 GU-N (SEBS) Compound
Description: Kraton G7820 GU-N is an easy processing, general purpose 90 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form..