Polymer Property : Tensile Strength = 325 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 325 MPa
47100 psi
ASTM D-638
PlastiComp Complet® LCF30-PES Polyethersulfone, 30% Long Carbon Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Polyethersulfone with 30% long carbon fiber reinforcementInformation provided by Plast..