Polymer Property : Tensile Strength = 338 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 338 MPa
49000 psi
ASTM D638
Quantum Composites AMC™ 8592 55% Carbon Fiber Reinforced SMC
AMC™ 8592 is a chopped carbon fiber reinforced engineered structural composite molding compound. It is easily moldable and provides parts that are high strength, fatigue resistant, with high heat ..