Polymer Property : Tensile Strength = 33900 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 234 MPa
33900 psi
ASTM D638
PlastiComp Complet® LBF50-PA66 50% Long Basalt Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Tensile Strength 234 MPa
33900 psi
ASTM D-638
PlastiComp Velocity® LGF50-PA6 High Flow Nylon 6, 50% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Tensile Strength 234 MPa
33900 psi
ASTM D638
Quantum Composites QC-8850 43% Glass Fiber Reinforced Polyester Hybrid SMC
QC-8850 is a polyester hybrid engineered structural composite molding compound designed for compression molding of components requiring high structural strength. It exhibits unusual toughness, and ..