Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 2.48 MPa @Strain 100 % |
360 psi @Strain 100 % |
510 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Flexible A55G0 Polyvinyl Chloride, Flexible (PVC, Flexible) Recommended for interior applications.Information provided by PolyOne |