Polymer Property : Tensile Strength = 379 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 379 - 483 MPa
55000 - 70000 psi
Eagle Brass 200/201 Nickel Alloy, 1/4 Hardened
Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick..
Tensile Strength >= 379 MPa
>= 55000 psi
Eagle Brass 200/201 Nickel Alloy, Annealed
Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick..
Tensile Strength 379 - 517 MPa
55000 - 75000 psi
Eagle Brass 1008 Low Carbon Steel, 1/2 Hardened
1008 is a standard grade Carbon Steel. This alloy is generally used for "commercial quality" cold rolled steel. It is an economical, general purpose steel grade offering moderate strength and toughn..