Mechanical Properties Metric English Comments
Tensile Strength 70.0 - 390 MPa
10200 - 56600 psi
MD
Quadrant Plastic Composites GMTex® Glass-Mat-Reinforced Thermoplastic
Based on GMT, the composite GMTex has been further developed for applications demanding high impact resistance, strength and durability. In the production of these high-performance thermoplastic co..