Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 272 MPa @Thickness 0.0178 mm |
39500 psi @Thickness 0.000701 in |
ASTM D882-02 |
NeXolve Novastrat® 800 Polyimide High temperature polyimide film with low coefficient of thermal expansion.NeXolve Novastrat® 800 is a high temperature polyimide film with low coefficient of thermal expansion (CTE), ~4 ppm/°C fro.. |