Polymer Property : Tensile Strength = 41200 psi
Polymer Property :
Tensile Strength =
41200 psi
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tensile Strength
284
MPa
41200
psi
ASTM D-638
PlastiComp Complet® LCF20/LGF20 – PA66 BLK Polyamide 66, 40% Long Carbon/Glass Fiber
Composite PelletsInformation provided by PlastiComp, Inc.