Mechanical Properties Metric English Comments
Tensile Strength 42.2 MPa
6120 psi
50 mm/min; ISO 527-1,-2
Gromax BTE70-FN001N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength 42.2 MPa
6120 psi
50 mm/min; ISO 527-1,-2
Gromax BTQ80-AQ00N1 Nylon 6, Impact Modified (Dry)
Information provided by Gromax Enterprises Corp.
Tensile Strength 42.2 MPa
6120 psi
50 mm/min; ISO 527-1,-2
Gromax BTE45-DN00N1 Nylon 6 (Dry)
Information provided by Gromax Enterprises Corp.