Tensile Strength 29.04 MPa
4212 psi
Cyclewood Solutions Xylomer™ XM2-JNA Sustainable Injection Molding Resin
100% biodegradable and compostable thermoplastic. The sustainable bio-based resin properties perform between polypropylene and polystyrene. Xylomer™ is modified lignin, an abundant, natural bypro..