Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 435 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 3.00 MPa
>= 435 psi
in the plane; ISO 527 1-2
3A Composites Core Materials AIREX® C70.130 Universal Structural Foam
AIREX® C70 is a closed cell, crosslinked polymer foam that combines excellent stiffness and strength to weight ratios with superior toughness. It is non-friable, contains no CFC’s, has negli..
Tensile Strength 3.00 MPa
435 psi
Momentive Performance Materials Siloprenâ„¢ LIM 6010 Liquid Silicone Rubber - Fast Cure / High Tear
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
Tensile Strength 3.00 MPa
435 psi
Momentive Performance Materials Siloprenâ„¢ LSR 2003 Liquid Silicone Rubber - General Purpose
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
Tensile Strength 3.00 MPa
435 psi
Momentive Performance Materials Siloprenâ„¢ LSR 2010 Liquid Silicone Rubber - General Purpose
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
Tensile Strength 3.00 MPa
435 psi
Momentive Performance Materials Siloprenâ„¢ LSR 2610 Liquid Silicone Rubber - Fast Cure / High Tear
This LSR elastomer is a general purpose, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera..
Tensile Strength 3.00 MPa
435 psi
Shin-Etsu Silicones KE-1204 BL Silicone, Potting/Encapsulation RTV
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 3.00 MPa

@Strain 100 %
435 psi

@Strain 100 %
ISO 37
BASF Elastollan 670 AWHU TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..