Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 46.8 MPa | 6790 psi | 7 Day Cure; ASTM D695 |
Protective Coating PC-Concrete™ Epoxy Concrete Anchoring and Repair System PC Concrete™ epoxy gel is an anchoring and concrete repair product. PC Concrete™ is formulated for anchoring threaded rods, bolts, rebar dowels and smooth dowels into concrete, grout filled block,.. |
|||
Tensile Strength | 46.8 MPa | 6790 psi | ASTM D 638 |
Saint-Gobain Meldin® 1380 Thermoplastic Bearing Material Specify Meldin 1380 for use with soft mating surfaces that gall easily, such as stainless steel or aluminum. Meldin 1380 also complies with the FDA Title 21 CFR regulations for contact with article.. |