Tensile Strength 3200 MPa
464000 psi
Kuraray Vectran® HT 1500/300 LCP Fiber
 is a high-performance multifilament yarn spun from liquid crystal polymer (LCP).  fiber exhibits exceptional strength and rigidity. Pound for pound  fiber is five times stronger than steel an..