Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 47.1 MPa | 6830 psi | ASTM D412 |
Kolon ELLAS K-470A Ester Based Thermoplastic Polyurethane ApplicationsInjectionIndustry PartsParts for Automobile/Mobile phoneABS Compound |
|||
Tensile Strength | 47.1 MPa | 6830 psi | ASTM D638 |
GRECO ISOPAK 547 ABS Resin High Impact GradeInformation provided by Greater Eastern Resins Industrial Co., Ltd. |
|||
Tensile Strength | 47.1 MPa | 6830 psi | |
Taiwan Sheen Soon Sheenthane® D6612R Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |