Tensile Strength 5.21 MPa

@Strain 100 %
755 psi

@Strain 100 %
ASTM D412
Lubrizol STAT-RITE® S-1107 Static Dissipative TPU
Description: Stat-Rite® S-1107 is a static dissipative TPU alloy. Stat-Rite S-1107 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD ..