Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 552 - 621 MPa | 80000 - 90000 psi | |
Chicago Extruded Metals BioBrass® UNS C64700 Copper-Silicon Alloy Finished product available as bar, wire, or rod.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extruded Meta.. |
|||
Tensile Strength | >= 552 MPa | >= 80000 psi | |
Eagle Brass 1008 Low Carbon Steel, Full Hardened 1008 is a standard grade Carbon Steel. This alloy is generally used for "commercial quality" cold rolled steel. It is an economical, general purpose steel grade offering moderate strength and toughn.. |