Polymer Property : Tensile Strength = 560 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 3.86 MPa
560 psi
Teknor Apex Elexar® EL 3954-45 Thermoplastic Elastomer
Notes: Elexar® is a family of styrene block copolymer thermoplastic elastomers, often referred to as thermoplastic rubber (TPR). Elexar® "rubber-like" compounds offer superior electrical prop..
Tensile Strength 3.86 MPa
560 psi
Silicone Property; ASTM D412
Arlon Thermabond® T-20 NP (99770W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: 8 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction: Liner: FEP Product: Uncured Silicone Ru..
Tensile Strength 3.86 MPa
560 psi
Silicone Property; ASTM D412
Arlon Thermabond® T-20 NP (99770W015) 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: 15 mil Primerless Thermabond®. T-20 NP. Thermally conductive, electrically insulating electronic adhesive. Bonds with primer.Design/Construction:Liner: FEPProduct: Uncured Silicone Rub..
Tensile Strength 3.86 MPa

@Strain 100 %
560 psi

@Strain 100 %
ASTM D638
Teknor Apex APEX® 3311-60NT Polyvinyl Chloride, Flexible
Features: Non-DEHP Plasticizer; Ethylene Oxide Sterilizable Uses: Medical/Healthcare Applications; Toys; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Teknor Apex