Mechanical Properties Metric English Comments
Tensile Strength 3.90 MPa
566 psi
Shin-Etsu Silicones LIMSâ„¢ KE1950-10A/B Elastomer
KE-1950-10 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy ..
Tensile Strength 3.90 MPa
566 psi
Shin-Etsu Silicones KE-1831 Silicone, RTV Adhesive/Sealant
Information Provided by Shin-Etsu Silicones of America, Inc.
Tensile Strength 3.90 MPa
566 psi
500 mm/min, measured parallel to flow; ISO 37
AlphaGary Evoprene™ LF 6151 Automotive Thermoplastic Elastomer
Evoprene™ LF is a hydrogenated styrene block copolymer based thermoplastic elastomer created for the automotive industry. It is specially formulated to have very low fogging characteristics suitab..
Tensile Strength 3.90 MPa
566 psi
ISO 37
AlphaGary Evoprene™ G 966 SEBS Thermoplastic Elastomer
Evoprene™ G compounds are styrene – ethylene butylene –styrene base thermoplastic elastomer with related hydrogenated block copolymers. These polymers are fully saturated so the resistance to oxi..