Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E831-28/16-Y-ERYB-LMP Cool Gray PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 760-35/1-IS-SD Ivory PVC Compound PVC compound for extrusion of monofilament.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 804-02/39-Y-RTC Blue PVC Compound Flame retardant PVC compound recommended for electrical conduit extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 804-48/1-CRE Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 805-10/127-A-ERYB-AS-PO White PVC Compound Weather resistant PVC powder compound recommended for extrusion in twin screw extruder of window and door profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 805-10/152-A-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 806-10/42-B-RT-PO White PVC Compound PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 806-18/364-BY-ERYB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 810-37/3-CRB Ocher PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 811-10/23-A-ERYB-PO White PVC Compound PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 813-35/1-DY-SN-ERYB Compound PVC Ivory Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 828-08/20-AY-ERYB-PO Beige PVC Compound PVC powder compound recommended for extrusion in twin screw extruder of door profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 837-35/1-A-ERYB-LMP Ivory PVC Compound Heavy metal free PVC compound recommended for extrusion of furniture profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina 851-10/127-Y-ERYB-AS-PO White PVC Compound Weather resistant PVC powder compound recommended for extrusion in twin screw extruder of window and door profiles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 76/205-IS-SD-TR Crystal PVC Compound Crystal PVC compound recommended for sleeves.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 800-35/1-B-ERB Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 811-10/184-Y-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 813-10/164-B-RT-PO White PVC Compound PVC powder compound, recommended for extrusion in twin screw extruder of sewer pipes.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 813-35/1-DY-SN-ERYB Compound PVC Ivory Ivory PVC compound recommended for extrusion of profiles developed for Teknaform Canada.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 818-35/1-Y-SN-ERM Ivory PVC Compound Tin stabilized PVC compound recommended for extrusion of rigid profilesInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 832-10/84-Y-ERM White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 835-10/156-C-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 835-18/115-C-ERYB Gray PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 837-10/168-A-ERYB-AS White PVC Compound With UV protectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 838-10/182-Y-ERYB White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 39.2 MPa | 5690 psi | 50 mm/min; ISO 527-1,-2 |
Gromax ATE90-FN01N1 Nylon 6 (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | >= 39.2 MPa | >= 5690 psi | ASTM D 638 |
Karina E 871-10/366-Y-ERYB White PVC Compound Rigid white PVC compound recommended for extrusion of profiles. Developed for Window City under GG3034 D70.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | 39.2 MPa | 5690 psi | |
Taiwan Sheen Soon Sheenthane® A8870E Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 39.2 MPa | 5690 psi | |
Taiwan Sheen Soon Sheenthane® A8871E2 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 39.2 MPa | 5690 psi | |
Taiwan Sheen Soon Sheenthane® A9550 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingPolyether gradeInformation provided by Taiwan Sheen Soon Co., LTD. |