Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina E CAK 60-48/1 Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina E CAK 65/48/1-CS Black PVC Compound Reclaimed PVC Compound.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina E550D06/957 Blue PVC Compound Shoe IndustryInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina E600D06/958 Light Blue PVC Compound Shoe IndustryInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina 500D48/1-A-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina 60/200 Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina 600D48/1-A-IS-BZ Black PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina 600-DA-48/1-C-IS Black PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina 920-10/156-Y-IS-BZ White PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina E 550D48/1 Black PVC Compound Shoe IndustryInformation provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina E 601D22/15 Crepe PVC Compound For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina E 605D06/476-AT Blue PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina E 650D35/1-C Ivory PVC Compound For footware/soles.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina E 704-35/1-J-IS Ivory PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina 600D18/136-A-IS-BZ Gray PVC Compound Heavy metal free PVC compound recommended for injection of automotive parts.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina E 60/200 Cristal Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Tensile Strength | >= 6.86 MPa | >= 996 psi | ASTM D 638 |
Karina E 60/200-D Clear PVC Compound Information provided by Karina Indústria e Comércio de Plásticos Ltda. |