Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 63.7 MPa | 9250 psi | 50 mm/min; ISO 527 |
Gromax BTG25-FN09N1 Nylon 6 25% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Strength | 63.7 MPa | 9250 psi | |
Taiwan Sheen Soon Sheenthane® A9313H Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 63.7 MPa | 9250 psi | |
Taiwan Sheen Soon Sheenthane® D6610 Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for injection moldingInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
Tensile Strength | 63.7 MPa | 9250 psi | ASTM D638 |
Samyang Trimma® FT6125 I[R] PMMA, Transparent High transparency and high scratch resistance. Stable against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang. |
|||
Tensile Strength | 63.7 MPa | 9250 psi | ASTM D638 |
Samyang Trirex® 3017PJ Polycarbonate PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017PJ is a super high flow grade.Information provided by Samyang. |
|||
Tensile Strength | 63.7 MPa | 9250 psi | ASTM D638 |
Samyang Trirex® 3017IR Polycarbonate with Heat Stabilizer PC is characterized by its excellent impact resistance, dimensional stability and excellent thermal resistance.3017IR is a super high flow grade with added heat stabilizers, separating materials and.. |
|||
Tensile Strength | 63.7 MPa | 9250 psi | ASTM D638 |
Samyang Triloy® 450N Polymer Alloy, Blow Molding Excellent impact, formability and weather resistance.450N is a blow molding grade.Applications: ConnectorsInformation provided by Samyang. |