Polymer Property : Tensile Strength = 6640 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength >= 45.8 MPa
>= 6640 psi
ASTM D 638
Karina E 830-35/1-Y-ERYB-LMP Ivory PVC Compound
Heavy metal free PVC compound recommended for extrusion of furniture profiles/.p>Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tensile Strength >= 45.8 MPa
>= 6640 psi
ASTM D 638
Karina E 854-35/9-A-ERYB Ivory PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.