Polymer Property : Tensile Strength = 6800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 46.9 MPa
6800 psi
ASTM D638
Quadrant EPP TIVAR® H.O.T. UHMW-PE, Premium Heat Stabilized/Anti-Oxidant Filled, (FDA, USDA, & 3-A Dairy) (ASTM Product Data Sheet)
Tensile Strength 46.9 MPa
6800 psi
ASTM D638
Techmer ES HiFill® TPX-PBT-98010 BN069
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityAppearance: Light BeigeProcessing Method: Injection MoldingInformation provided by TP C..
Tensile Strength 46.9 MPa
6800 psi
ASTM D638
Ensinger Tecatron® XP-74 Compression Molded PPS Compound, with 30% Carbon Fiber and 8% PTFE
Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p..
Tensile Strength 46.9 MPa
6800 psi
ASTM D638
Americas Styrenics STYRON® 693 High Heat Crystal Polystyrene
Product CharacteristicsHigh heat resistanceHigh tensile strengthHigh stiffnessFood Contact CompliantUL Classification 94 HBTypical ApplicationsPackaging/Foam disposablesConsumer electronicsInformati..
Tensile Strength 46.9 MPa
6800 psi
ASTM D638
Aaron Industries AAROPRENE® GFIPP 2020 High Impact Glass Filled Polypropylene
AAROPRENE® GFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.