Polymer Property : Tensile Strength = 7.453 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 7.453 MPa
1081 psi
Silicone Property; ASTM D412
Arlon 32210A005 0.005" (0.127 mm) Uncured Fluorosilicone Rubber on Polyester Carrier
Design/Construction: Interleave: PolyethyleneSide 1: Uncured Fluorosilicone RubberCarrier: PolyesterThis data represents typical values for the production material. The data should not be used to wr..