Polymer Property : Tensile Strength = 7.481 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 7.481 MPa
1085 psi
Silicone Property; Arlon SQA-TMS-008
Arlon 51044R020 0.020" Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Semi-cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should no..
Tensile Strength 7.481 MPa
1085 psi
Silicone Property; ASTM D412
Arlon 51112R013 0.013" (0.330 mm) Cured, Self Fusing, Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured, Self Fusing, Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material. The data sho..
Tensile Strength 7.481 MPa
1085 psi
Silicone Property; ASTM D412
Arlon 910-10X##-P1 0.010" (0.254 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 10 mil thick, Gray, Rectangular cross-section, Self-fus..
Tensile Strength 7.481 MPa
1085 psi
Silicone Property; ASTM D412
Arlon 940-15R##-P0 0.040" (1.02 mm) Cured Self-fusing Silicone Tape
Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1.5” Wide Rectangular 1.5 inch wide, 40 mil thick, Red, Rectangular cross-section, Self-f..