Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength = 7256 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 50.03 MPa
7256 psi
ASTM D-412
Lubrizol Advanced Materials Pearlthane® 11T75D Thermoplastic Polyurethane Elastomer
Pearlthane® 11T75D is a polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, with extremely high hardness. It is especially recommended for use in producin..