Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 517 - 586 MPa | 75000 - 85000 psi | Plate and Rounds |
IBC Advanced Alloys C18150 Chrome Copper Zirconium Alloy, TL06 Temper C18150 Chrome Copper Zirconium is recommended for spot and seam welding cold and hot-rolled steel, stainless steel and low conductivity brass and bronze. C18150 Chrome Copper Zirconium Alloy is typi.. |
|||
Tensile Strength | >= 517 MPa | >= 75000 psi | |
Eagle Brass 301 Austenitic Stainless Steel, Annealed Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tens.. |
|||
Tensile Strength | >= 517 MPa | >= 75000 psi | |
Eagle Brass 302 Austenitic Stainless Steel, Annealed Types 302 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |
|||
Tensile Strength | >= 517 MPa | >= 75000 psi | |
Eagle Brass 316 Austenitic Stainless Steel, Annealed The Mo addition increases general corrosion resistance to pitting from chloride ion solutions, and provides increased strength at elevated temperatures. Properties are similar to those of Type 304 .. |
|||
Tensile Strength | 517 - 676 MPa | 75000 - 98000 psi | |
Chicago Extruded Metals BioBrass® UNS C62300 Aluminum Bronze Finished product available as bar, rod, forged or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Extr.. |
|||
Tensile Strength | 517 - 703 MPa | 75000 - 102000 psi | |
Chicago Extruded Metals BioBrass® UNS C64200 Aluminum Bronze Finished product available as bar, rod, forged, or shapes.Chicago Extruded Metal temper codes: H02, M30This alloy is registered with the U.S. EPA as Antimicrobial.Information provided by Chicago Ext.. |
|||
Tensile Strength | >= 517 MPa | >= 75000 psi | |
Eagle Brass 304 Austenitic Stainless Steel, Annealed Types 304 is a widely used variation of the basic 18-8 grade with variations of nickel, chromium and carbon content. It is weakly magnetic when cold rolled.Information provided by Eagle Brass Compa.. |