Polymer Property : Tensile Strength = 761 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength 5.25 MPa
761 psi
ASTM D412
Elastocon TPE Technologies Elastocon® 8150B Thermoplastic Elastomer
Elastocon® 8150B is a black thermoplastic elastomer formulated for applications that require rubber-like properties and a good surface finish. Elastocon® 8150B is well suited for consumer goods a..